top of page

CFA Series

IMG_6336-4-finall.png
Product Description

CFA is made by soaking and drying huge foamed pyramid foam with raw materials. The size and number of pyramids can be adjusted according to the reflection loss (db) value.

1. PU foam absorber

2. Easy to break when bent

​3. Adaptation temperature -20℃~80℃

Product specifications
浮水印-網頁用-CFA-規格表.png
CFA規格.jpg
Product test method
​Measurement method

According to the microwave anti-wave reflection attenuation and measurement method customized by our laboratory, this method refers to the method in the appendix [1] of the US military regulation MIL-A-17161D* (the measurement method is not the direct transmission of the signal and the direct absorption contact)

 

Measurement range 3~18GHz reflection attenuation characteristics (expressed by db loss value)

 

Generally speaking, -3db means 50% absorption, -6db means 75% absorption, -10db means 90% absorption, -20db means 99% absorption.

​Measuring Instruments

HP8500B Vector Network Analyzer

​Measurement unit

The product of the microwave reflection attenuation measurement report of the Microwave Measurement Laboratory of the Institute of Chemistry, Zhongshan Academy of Sciences, Taiwan